Investigation of High Energy Single Pulse Effect on Micro Arc Oxidation (MAO) Process on Aluminium

Thumbnail

Göster/Aç

Ana makale (978.6Kb)

Erişim

info:eu-repo/semantics/openAccess

Tarih

2019

Yazar

Yılmaz, Mustafa Safa
Şahin, Orhan

Üst veri

Tüm öğe kaydını göster

Künye

YILMAZ, Mustafa Safa & Orhan ŞAHİN. "Investigation of High Energy Single Pulse Effect on Micro Arc Oxidation (MAO) Process on Aluminium". International Journal of Mining, Materials, and Metallurgical Engineering (IJMMME), 5 (2019): 1-6.

Özet

Micro Arc Oxidation (MAO) was applied by using high-energy anodic/cathodic pulses with various pulse durations. Anodic and cathodic pulse couples were kept at a constant voltage of 500 volts. Energy of each pulse increased with increasing duration of pulses. Since the aim of the present study was to investigate effect of pulse durations on MAO processing, other processing parameters such as duty cycle (8%), electrolyte temperature (25±5 °C), electrolyte composition (KOH, Na2SiO3.5H2O), process time (20 minutes), anodic pulse voltage, cathodic pulse voltage and chemical composition of substrate were all kept constant. Five different anodic and cathodic pulse durations were applied. Scanning electron microscope (SEM), indenter, profilometer, eddy current and X-ray diffractometer were employed to investigate the microstructure, hardness, surface roughness, coating thickness and phase distribution of the coatings. Varying of pulse duration occurred significant differences among coating specifications. Coating layers with thickness between 50-90 μm and surface roughness between 3.1-5.2 μm were obtained. The hardness of coating layers was between 800-2000 Vickers. Coatings consist of two sub-layers, inner dense layer and outer porous layer, which were a mixture of γ-Al2O3 and α- Al2O3.

Kaynak

International Journal of Mining, Materials, and Metallurgical Engineering (IJMMME)

Cilt

5

Bağlantı

https://ijmmme.avestia.com/2019/PDF/001.pdf
https://hdl.handle.net/11352/3474

Koleksiyonlar

  • Alüminyum Test Eğitim ve Araştırma Merkezi (ALUTEAM) [118]
  • Scopus İndeksli Yayınlar / Scopus Indexed Publications [630]



DSpace software copyright © 2002-2015  DuraSpace
İletişim | Geri Bildirim
Theme by 
@mire NV
 

 




| Politika | Rehber | İletişim |

DSpace@FSM

by OpenAIRE
Gelişmiş Arama

sherpa/romeo

Göz at

Tüm DSpaceBölümler & KoleksiyonlarTarihe GöreYazara GöreBaşlığa GöreKonuya GöreTüre GöreDile GöreBölüme GöreKategoriye GöreYayıncıya GöreErişim ŞekliKurum Yazarına GöreBu KoleksiyonTarihe GöreYazara GöreBaşlığa GöreKonuya GöreTüre GöreDile GöreBölüme GöreKategoriye GöreYayıncıya GöreErişim ŞekliKurum Yazarına Göre

Hesabım

GirişKayıt

İstatistikler

Google Analitik İstatistiklerini Görüntüle

DSpace software copyright © 2002-2015  DuraSpace
İletişim | Geri Bildirim
Theme by 
@mire NV
 

 


|| Politika || Rehber || Kütüphane || FSM Vakıf Üniversitesi || OAI-PMH ||

FSM Vakıf Üniversitesi, İstanbul, Türkiye
İçerikte herhangi bir hata görürseniz, lütfen bildiriniz:

Creative Commons License
FSM Vakıf Üniversitesi Institutional Repository is licensed under a Creative Commons Attribution-NonCommercial-NoDerivs 4.0 Unported License..

DSpace@FSM:


DSpace 6.2

tarafından İdeal DSpace hizmetleri çerçevesinde özelleştirilerek kurulmuştur.